Laser welding technology has become a cornerstone in the fields of manufacturing and engineering, offering precision and efficiency unmatched by traditional methods. However, mastering this technique requires understanding and addressing its common pitfalls. We've consulted with industry experts to bring you five essential solutions to the most common laser welding defects.
1. Hot Cracking

"Hot cracking is a challenge that tests the skill of every laser welding technician. The key to preventing it lies in understanding the material's behavior under heat," explains Dr. Emily Zhao, a materials scientist with over 15 years of experience in laser welding research.
Solution: Utilize filler wire and preheat the material. Filler wire compensates for material lost to evaporation and shrinkage, while preheating moderates the cooling rate, reducing stress.
2. Porosity


"Porosity can be the bane of a perfect weld, often hidden until a critical failure occurs," states Michael Chen, a senior laser welding engineer. "Prevention is all about control—controlling your materials and your environment."
Solution: Clean the workpiece thoroughly before welding and adjust the shielding gas flow to ensure gases are expelled from the molten pool effectively.
3. Spatter

According to Alex Rivera, a welding technician with a decade of experience, "Spatter might seem minor, but it can significantly affect a product's finish and, in some cases, its functionality."
Solution: Reduce power density to minimize spatter. Adjusting welding parameters like speed and energy input can also help control the molten pool's behavior.
4. Undercut

"Undercut is often a sign of rushing. It's a reminder that speed must be balanced with quality," remarks Liu Wei, a project manager specializing in laser fabrication.
Solution: Carefully control the welding speed and ensure the assembly gap is appropriate. This allows the molten metal to distribute evenly, avoiding the formation of undercuts.
5. Collapse and Pits

Sophie Patel, a quality assurance analyst, emphasizes the importance of aesthetics and integrity in welding. "Collapses and pits not only mar the surface but can also introduce weak points in the weld," she says.
Solution: Lowering the energy density and adjusting the welding speed can prevent excessive molten pool depth, maintaining the weld's integrity and appearance.